It elucidated the typical hexagonal structure for ZnO and spinel cubic structure for ZnFe2O4 with an average crystallite of 31 nm and 44 nm for ZnO and ZnFe2O4, respectively. The micrographs obtained by SEM showed rough spherical particles of ZnO, whereas for ZnFe2O4 flower-like clustered particles were observed. The photocatalytic investigation against diclofenac sodium revealed the higher degradation efficiency of ZnFe2O4 (61.4%) in only 120 min, whereas ZnO degraded only 48.9% of the drug. Moreover, zinc ferrite has shown good rec